PRINCIPAL ELEMENTS %
 
Ni
-
Cr
28.5
Mo
6
Ma
-
Mg
<1
Al
-
Be
-
Ti
-
Si
<1
Co
63
Fe
-
W
-
C
-
Other
-
MELTING RANGE °C
1388 ~ 1431
CASTING TEMP °F
2525
TENSILE STRENGTH  Mpa
834
YIELD STRENGTH %
663
TENSILE ELONGATION %
6
DENSITY g/ cm³
8.3
SPECIFIC GRAVITY g/cm³
-
LINIER EXPANSION ppm/C
-
BRINNEL HARDNESS
-
VICKERS HARDNESS HV
363
ULTIMATE STRENGTH Psi
123
MSDS

 

Instructions for use: 

Dream Cast Chrome

Partial Denture Casting Alloy

Chrome-Cobalt

 Processing Technique:

Investment:

Use investment recommended by manufacturers only for high heat Crhomium-Cobalt Partial Denture Alloy. Follow the manufacturer’s instructions carefully.

 

Torch Casting:

1-     Multi-orifice tips are recommended.

2-     Set gauges to 20 psi oxygen and 8 psi acetylene.

3-     Light the torch; for better results allow the blue inner flame expand not more than 1/8” (3mm), and the outer flame approximately 1 ½” (38mm) from the torch tip.

4-     Place sufficient alloy in the preheated crucible.

5-     Heat the alloy uniformly. Cast immediately after slumping to avoid excessive burning.

Induction Casting:

Follow the manufacturer’s instructions; set the temperature to 2700ºF (1480ºC). When the metal has melted as one mass; release the machine immediately to avoid overheating.

Finishing:

1-     Use thin cut-off wheels to remove buttons by cutting sprues close to the casting and trim remaining metal from sprues and shape with heavy cut-off wheels.

2-     Use barrel shape stones to grind the surface of lingual and balatal bars, and shape the finish line areas on the upper cases.

3-     Use inverted cone type stones to trim or grind tight areas.

4-     Do not stone stippled surfaces, electro polish the high stone.

5-     Casting should be ready for sandblasting and polishing.

Electro Polishing:

Use electro polishing units that are recommended for high heat Chromium-Cobalt Partial Denture Alloys. Follow the manufacturer’s instructions; remove the case from the solution and rinse thoroughly with running water; go over entire case and remove all surface marks with rubber wheels and points.

Welding & Soldering:

1-     Clean by grinding or sandblasting the surface of the areas and then invest.

2-     Thick areas should be ground to shape so that the top of the surface is wider than the bottom.

3-     Adjust the torch to one (1) psi oxygen and one (1) psi acetylene.

4-     After lighting the torch adjust to neutral flame with approximately ½” (12mm) blue cone extending from the torch tip.

5-     Heat the welding rod and slip it into the flux, heat both parts of welding areas.

6-     Clean the case in an ultrasonic cleaner.

Recommended Solder: Use cobalt based dental solder recommended by solder’s manufacturer.

Note: For best results use at least 50% new metal with 50% sandblasted and cleaned buttons.

 

Caution: Federal Law restricts this device to sale by or on the order of a dentist!

This product was added to our catalog on Friday 06 October, 2006.
Reviews
Categories
Alloys (5)
Etc
Handpieces (13)
Lab (11)
Micromotors (6)
Osseo (2)
Products (7)
 
 New Product
 Specials
 
Featured more
COMPRESS & DENTURE FLASKS
COMPRESS & DENTURE FLASKSdd
Registered user ONLY
Copyright © 2010 America Green Dent Mfg.
Webmaster: Dennis Chung
  Wednesday 08 September, 2010     65461 requests since Wednesday 04 October, 2006